Examples
- The optimum conditions for air electrode preparation were shown as follow : 20 % ptfe and 20 % mno2 in active layer , thickness of active layer 0 . 15 - 0 . 25mm and the ratio of active carbon to ethine black 4 : 1 ; 60 % ptfe in the gas diffusion and waterproof layer , employing na2so4 as pore - making agents , thickness 0 . 35 - 0 . 45mm , colding forming and layer sequence catlytic layer / gas diffusion and waterproof layer / current collector layout ; employing 40 meshed nickel screen as current collector and thermal treatment temperature over 200